Nickel alloy 188 is a cobalt-base alloy that offers good resistance to oxidation to 2000°F and excellent high temperature strength. The alloy also has good sulfidation resistance, excellent metallurgical stability, and good ductility after prolonged exposure to temperatures of 760-871.1°C (1400-1600°F). It has good ductility.
Alloy 600 and 625 resists steam and mixtures of steam, air, and carbon dioxide. The alloy has excellent oxidation resistance to about 2100 °F (1149 °C). This series of alloys is well-known for its performance in extreme heat conditions—which makes each alloy variant extremely popular for use in furnace applications such as heat treating or […]
L605 is a cobalt-chromium-tungston-nickel alloy.L605 displays excellent high-temperature strength and excellent oxidation resistance to 2000°F. The material also has good sulfidation resistance and resistance to wear and galling. It is non-magnetic. The high chromium content makes it resistant to corrosion in a wide range of environments such as wet chlorine, hydrochloric acid and nitric acid. […]
Monel® K500 is a nickel-copper alloy with increased properties obtained by adding aluminum and titanium and by age hardening. Alloy K-500 has approximately three times the yield strength and double the tensile strength when compared with alloy 400. Plus, it can be further strengthened by cold working prior to precipitation hardening. The strength of this […]
Reviews
There are no reviews yet.